Knowledge Center

A:

This is a very valid concern. The shoulder is injection-molded onto the tube body at over 200°C, but the bond strength between them is tested under ambient conditions. If you fill with a 60°C product, the HDPE material in the shoulder softens significantly, and the axial load applied during the capping process (usually 15–25 N) can cause shoulder delamination.
To prevent this, we don't just rely on standard room-temp QC. If you tell us it's a warm fill, we will run an elevated-temperature pull test (simulating your 60°C fill and capping load) on the production batch. We can also adjust the shoulder overlap depth to be at least 4.0–6.0 mm to give it more mechanical grip. Warm fills are a common cause of failure, but with the right spec from the start, it's easily solved.

A:

Side seam splitting (delamination) during filling is usually caused by three factors: 1. Heat sealing parameters (temperature, pressure, or dwell time are not matched to the laminate structure), 2. Seal zone contamination (tiny amounts of paste or oil trapped in the seam before sealing), or 3. Incompatible resin (the inner PE layer is too thin). If your line is running too hot to compensate for speed, the PE layer can degrade and become brittle. Always verify the recommended sealing window provided by your tube manufacturer and check for product splash.